Phase Formation and Microhardness ...

Phase Formation and Microhardness Distribution in the Transition Zone Between Titanium and Nickel Alloys Fabricated by Wire Arc Additive Manufacturing

Researchers from the laboratories of Structural Design of Advanced Materials and Surface Hardening Physics at the Institute of Strength Physics and Materials Science SB RAS have investigated the formation of microstructure, phase composition, and microhardness distribution in the transition zone between Ti–6Al–4V–2Zr–2Mo titanium alloy and Inconel-625 nickel-based superalloy fabricated by wire arc additive manufacturing.
Using scanning electron microscopy and X-ray diffraction analysis, it was established that sequential changes in phase composition occur within the ~10 mm thick transition zone, driven by variations in the local chemical composition. A sequence of phase formation was identified, ranging from a nickel-based γ-solid solution and TCP phases to structures containing η-Ni₃Ti and NiTi intermetallics, M₆C carbides, and Ti₂Ni near the titanium alloy interface. It was shown that the morphology of η-Ni₃Ti evolves from acicular to lamellar, eutectic, and bulk forms depending on the local Ti/Al ratio and cyclic thermal effects during additive manufacturing. The maximum microhardness of the transition zone reaches ~8 GPa in regions enriched with η-Ni₃Ti and TCP phases. The potential brittleness of these regions represents a significant factor in assessing the operational reliability of the joint. The obtained results demonstrate the possibility of regulating the phase composition and properties of the transition zone by controlling the local chemical composition of the material.
This research was funded by Government research assignment for ISPMS SB RAS, project FWRW-2024-0001. The research results were published in the journal Materials Letters (Q2 according to SJR): Vorontsov, A.; Tarasov, S.; Panfilov, A.; Eliseev, A.; Cheremnov, A.; Knyzhev, E.; Zykova, A. Microstructural Evolution, Phase Formation, and Microhardness in the Ti–6Al–4 V–2Zr–2Mo / Inconel-625 Transition Zone Fabricated by WAAM. Mater. Lett. 2027, 427, 141770, https://doi.org/10.1016/j.matlet.2026.141770 .

previous page